激光多次熔凝Zr55Cu30Al10Ni5非晶合金的晶化形态与演化机理
杨高林1,林鑫2(),卢献钢1
Crystallization Morphology and Evolution Mechanism of Laser Multiple Remelting of Zr55Cu30Al10Ni5 Metallic Glass
YANG Gaolin1,LIN Xin2(),LU Xiangang1

图2. 激光熔凝1、3、7和13次No.C非晶合金板后的熔池形貌OM像

Fig.2. OM images of No.C metallic glass plate after different times remelting(a) 1 time (b) 3 times (c) 7 times (d) 13 times