碳纳米管(CNTs)增强AZ91镁基复合材料组织与力学性能研究
覃嘉宇1,2,李小强1,2,金培鹏1,2,王金辉1,2,朱云鹏1,2,3()
Microstructure and Mechanical Properties of Carbon Nanotubes (CNTs) Reinforced AZ91 Matrix Composite
QIN Jiayu1,2,LI Xiaoqiang1,2,JIN Peipeng1,2,WANG Jinhui1,2,ZHU Yunpeng1,2,3()

图5. 挤压态AZ91基体合金和0.1%CNTs/AZ91复合材料的{0001}面和{101ˉ0}面宏观织构

Fig.5. {0001} and {101ˉ0} pole figures of as-extruded AZ91 alloy (a) and CNTs/AZ91 composite (b) (ED—extruded direction, TD—transverse direction)