[an error occurred while processing this directive]
碳纳米管(CNTs)增强AZ91镁基复合材料组织与力学性能研究
覃嘉宇1,2,李小强1,2,金培鹏1,2,王金辉1,2,朱云鹏1,2,3()
Microstructure and Mechanical Properties of Carbon Nanotubes (CNTs) Reinforced AZ91 Matrix Composite
QIN Jiayu1,2,LI Xiaoqiang1,2,JIN Peipeng1,2,WANG Jinhui1,2,ZHU Yunpeng1,2,3()

图6. 挤压态AZ91合金及0.1%CNTs/AZ91复合材料的室温压缩性能和室温拉伸性能

Fig.6. Compressive (a) and tensile (b) stress-strain curves of as-extruded AZ91 alloy and 0.1%CNTs/AZ91 composite