碳纳米管(CNTs)增强AZ91镁基复合材料组织与力学性能研究
覃嘉宇1,2,李小强1,2,金培鹏1,2,王金辉1,2,朱云鹏1,2,3()
Microstructure and Mechanical Properties of Carbon Nanotubes (CNTs) Reinforced AZ91 Matrix Composite
QIN Jiayu1,2,LI Xiaoqiang1,2,JIN Peipeng1,2,WANG Jinhui1,2,ZHU Yunpeng1,2,3()

图3. 挤压态AZ91基体合金和0.1%CNTs/AZ91复合材料的TEM像及晶粒尺寸分布

Fig.3. TEM images (a, c) and grain size distributions (b, d) of as-extruded AZ91 alloy (a, b) and 0.1%CNTs/AZ91 composite (c, d) (DRX—dynamic recrystallization)