碳纳米管(CNTs)增强AZ91镁基复合材料组织与力学性能研究
覃嘉宇1,2,李小强1,2,金培鹏1,2,王金辉1,2,朱云鹏1,2,3()
Microstructure and Mechanical Properties of Carbon Nanotubes (CNTs) Reinforced AZ91 Matrix Composite
QIN Jiayu1,2,LI Xiaoqiang1,2,JIN Peipeng1,2,WANG Jinhui1,2,ZHU Yunpeng1,2,3()

图4. CNTs及Mg17Al12在0.1%CNTs/AZ91复合材料中的分布及界面微观组织

Fig.4. Distribution of CNTs and Mg17Al12 in 0.1%CNTs/AZ91composite (a) and interfacial microstructure between CNTs and AZ91 (b)