[an error occurred while processing this directive]
碳纳米管(CNTs)增强AZ91镁基复合材料组织与力学性能研究
覃嘉宇1,2,李小强1,2,金培鹏1,2,王金辉1,2,朱云鹏1,2,3()
Microstructure and Mechanical Properties of Carbon Nanotubes (CNTs) Reinforced AZ91 Matrix Composite
QIN Jiayu1,2,LI Xiaoqiang1,2,JIN Peipeng1,2,WANG Jinhui1,2,ZHU Yunpeng1,2,3()

图1. AZ91镁合金粉末和CNTs微观组织

Fig.1. Morphologies of raw AZ91 alloy powders (a) and carbon nanotubes (CNTs) (b) (Inset in Fig.1b shows the SAED pattern of CNTs)