碳纳米管(CNTs)增强AZ91镁基复合材料组织与力学性能研究
|
|
覃嘉宇,李小强,金培鹏,王金辉,朱云鹏
|
Microstructure and Mechanical Properties of Carbon Nanotubes (CNTs) Reinforced AZ91 Matrix Composite
|
|
Jiayu QIN,Xiaoqiang LI,Peipeng JIN,Jinhui WANG,Yunpeng ZHU
|
|
| 表1 相关镁基复合材料室温力学性能[7,11,18,19,33,34] |
| Table 1 Mechanical properties of this work with other reported Mg matrix composites[7,11,18,19,33,34] |
|
Material | Tensile | R | Compressive | Ref. |
|---|
| σb / MPa | σ0.2 / MPa | δ / % | σbc / MPa | σ0.2 / MPa | δ / % | |
|---|
0.6%(CNTs+GNPs)/ Mg-1Al | 234 | 185 | 16.4 | 26.4 | - | - | - | [7] | | 1%AlN/AZ91 | 168 | 144 | 7.6 | 32.4 | - | - | - | [11] | | 1%CNTs/AZ91 | 389 | 278 | 12.8 | 30.3 | - | - | - | [18] | | 0.5%CNTs/AZ91 | 230 | 129 | 8 | 13.9 | - | - | - | [19] | | 1%CNTs/Mg-6Zn | 321 | 209 | 17 | 25.5 | - | - | - | [33] | | 2Y/AZ91 | 323.1 | 216.9 | 14.3 | 5.1 | - | - | - | [34] | | AZ91 | 376 | 332 | 10.3 | - | 567 | 415 | 14.2 | This work | | 0.1%CNTs/AZ91 | 393 | 352 | 9.3 | 44.68 | 617 | 445 | 15.5 | This work |
|
|
|