大尺寸单晶叶片中小角度晶界的形成与演化
|
|
Formation and Evolution of Low Angle Grain Boundary in Large-Scale Single Crystal Superalloy Blade
|
|
图11. 从小角晶界起始位置沿生长方向往上约5 mm位置处的取向分布 |
Fig.11. Distribution of orientation at the site which is about 5 mm from the initial site of low angle grain boundary along the upward growth direction |
![]() |