籽晶制备及Ti-47Al合金PST晶体取向控制
|
|
Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy
|
|
图6. Ti-47Al PST晶体纵剖面组织形貌 |
Fig.6. Ti-47Al PST crystals grown from the ultimate seed(a) macrostructure of the longitudinal section(b~g) microstructures of the seed after seeding process (b), the transition region (c), the stray grains in the transition region (d, e), the main body (f) and γ phase near the quench zone (g) corresponding to the boxes in Fig.6a |
![]() |