AZ31镁合金拉伸扭折带结构的产生及交互作用机制
周博1,2,隋曼龄1,2()
Generation and Interaction Mechanism of Tension Kink Band in AZ31 Magnesium Alloy
ZHOU Bo1,2,SUI Manling1,2()

图6. 拉伸扭折带与{101ˉ1}孪晶交互作用机理示意图

Fig.6. Schematics of deformation structures(a) interaction between tension kink band and {101ˉ1} twin (b) kink band (c) {101ˉ1} twin