[an error occurred while processing this directive]
AZ31镁合金拉伸扭折带结构的产生及交互作用机制
周博1,2,隋曼龄1,2()
Generation and Interaction Mechanism of Tension Kink Band in AZ31 Magnesium Alloy
ZHOU Bo1,2,SUI Manling1,2()

图5. 拉伸扭折带形成机理示意图

Fig.5. Schematics of the tension kink band formation mechanism(a) generation of dislocation pairs in initial structure (F indicate the force direction)(b) formation of K1 (α1 is the angle between the interface of K1 and the basal plane of matrix. The inset shows the orientation between the matrix and kink band under the external force)(c) interaction of K1 and K2 (α2 is the angle between the interface of K2 and the basal plane of matrix)