[an error occurred while processing this directive]
AZ31镁合金拉伸扭折带结构的产生及交互作用机制
周博1,2,隋曼龄1,2()
Generation and Interaction Mechanism of Tension Kink Band in AZ31 Magnesium Alloy
ZHOU Bo1,2,SUI Manling1,2()

图3. 扭折带交互作用区域的TEM分析

Fig.3. TEM analyses of the interaction of kink bands(a) TEM image of the interaction area (Subscript M indicates matrix)(b~e) SAED patterns of different areas in Fig.3a