两步贝氏体转变对中碳微纳结构钢韧性的影响
万响亮1,胡锋1,2,3(),成林2,3,黄刚2,3,张国宏2,3,吴开明1,2,3
Influence of Two-Step Bainite Transformation on Toughness in Medium-Carbon Micro/Nano-Structured Steel
WAN Xiangliang1,HU Feng1,2,3(),CHENG Lin2,3,HUANG Gang2,3,ZHANG Guohong2,3,WU Kaiming1,2,3

图8. 中碳钢两步贝氏体转变组织的TEM像

Fig.8. TEM images of medium-carbon steel for two-step bainitic transformations (Area of dashed lines show block RA/M)(a) new micro/nano-size bainitic-ferrite(b) nano-size martensite