TRIP型双相不锈钢Fe-19.6Cr-2Ni-2.9Mn-1.6Si在循环变形条件下的力学特性
|
|
Mechanical Characteristics of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si During Cyclic Deformation
|
|
图9. Fe-19.6Cr-2Ni-2.9Mn-1.6Si的循环应力-应变曲线 |
Fig.9. Cyclic stress-strain curves of Fe-19.6Cr-2Ni-2.9Mn-1.6Si steel (εap1—εap corresponding to transition of A→B, εap2—εap corresponding to transition of B→C or/and I→II)(a) σa-εa curve and σE-εE curve(b) σa-εap curves of Fe-19.6Cr-2Ni-2.9Mn-1.6Si steel and 329 DSS[ |
![]() |