TRIP型双相不锈钢Fe-19.6Cr-2Ni-2.9Mn-1.6Si在循环变形条件下的力学特性
|
|
Mechanical Characteristics of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si During Cyclic Deformation
|
|
图4. Fe-19.6Cr-2Ni-2.9Mn-1.6Si钢在增级循环加载实验中各应变幅循环稳定的迟滞回线 |
Fig.4. Stabilized hysteresis loops of Fe-19.6Cr-2Ni-2.9Mn-1.6Si steel at each strain amplitude in the ascend test |
![]() |