TRIP型双相不锈钢Fe-19.6Cr-2Ni-2.9Mn-1.6Si在循环变形条件下的力学特性
|
|
Mechanical Characteristics of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si During Cyclic Deformation
|
|
图3. Fe-19.6Cr-2Ni-2.9Mn-1.6Si钢在单级循环加载实验下迟滞回线随循环周次的变化 |
Fig.3. The change of hysteresis loops of Fe-19.6Cr-2Ni-2.9Mn-1.6Si steel with the number of cycles (N) at different strain amplitudes (εa)(a) εa=0.3% (b) εa=0.7% (c) εa=1.0% |
![]() |