TRIP型双相不锈钢Fe-19.6Cr-2Ni-2.9Mn-1.6Si在循环变形条件下的力学特性
陈雷1,2,郝硕2,邹宗园2,韩舒婷2,张荣强2,郭宝峰2()
Mechanical Characteristics of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si During Cyclic Deformation
CHEN Lei1,2,HAO Shuo2,ZOU Zongyuan2,HAN Shuting2,ZHANG Rongqiang2,GUO Baofeng2()

图1. Fe-19.6Cr-2Ni-2.9Mn-1.6Si钢的初始组织及疲劳试样示意图

Fig.1. Initial microstructure (a) and schematic of sample (unit: mm) (b) of Fe-19.6Cr-2Ni-2.9Mn-1.6Si steel