[an error occurred while processing this directive]
TRIP型双相不锈钢Fe-19.6Cr-2Ni-2.9Mn-1.6Si在循环变形条件下的力学特性
陈雷1,2,郝硕2,邹宗园2,韩舒婷2,张荣强2,郭宝峰2()
Mechanical Characteristics of TRIP-Assisted Duplex Stainless Steel Fe-19.6Cr-2Ni-2.9Mn-1.6Si During Cyclic Deformation
CHEN Lei1,2,HAO Shuo2,ZOU Zongyuan2,HAN Shuting2,ZHANG Rongqiang2,GUO Baofeng2()

图2. 单调加载时Fe-19.6Cr-2Ni-2.9Mn-1.6Si钢的工程应力-工程应变曲线和真应力-真应变及加工硬化率曲线