位错密度梯度结构Cu单晶微柱压缩的三维离散位错动力学模拟
熊健1,魏德安1,陆宋江1,阚前华1,康国政1,张旭1,2()
A Three-Dimensional Discrete Dislocation Dynamics Simulation on Micropillar Compression of Single Crystal Copper with Dislocation Density Gradient
XIONG Jian1,WEI Dean1,LU Songjiang1,KAN Qianhua1,KANG Guozheng1,ZHANG Xu1,2()

图10. 位错密度梯度结构模型沿Z轴加载时,位错密度不同的各层塑性应变及位错密度随应变的变化

Fig.10. The evolutions of plastic strain (a) and the dislocation density (b) in bottom, middle and top layer, which have different dislocation densities, when loading direction is along Z-axis which is parallel with the dislocation density gradient direction