[an error occurred while processing this directive]
位错密度梯度结构Cu单晶微柱压缩的三维离散位错动力学模拟
熊健1,魏德安1,陆宋江1,阚前华1,康国政1,张旭1,2()
A Three-Dimensional Discrete Dislocation Dynamics Simulation on Micropillar Compression of Single Crystal Copper with Dislocation Density Gradient
XIONG Jian1,WEI Dean1,LU Songjiang1,KAN Qianhua1,KANG Guozheng1,ZHANG Xu1,2()

图6. 位错密度梯度结构模型沿着X轴方向加载时在不同应变时表面的塑性应变分布

Fig.6. Distributions of plastic strain on the surface corresponding to strains of 0.05% (a), 0.10% (b), 0.15% (c), 0.20% (d) and 0.25% (e) in the compression process along the X-axis direction which is perpendicular to the dislocation density gradient directionColor online