[an error occurred while processing this directive]
位错密度梯度结构Cu单晶微柱压缩的三维离散位错动力学模拟
熊健1,魏德安1,陆宋江1,阚前华1,康国政1,张旭1,2()
A Three-Dimensional Discrete Dislocation Dynamics Simulation on Micropillar Compression of Single Crystal Copper with Dislocation Density Gradient
XIONG Jian1,WEI Dean1,LU Songjiang1,KAN Qianhua1,KANG Guozheng1,ZHANG Xu1,2()

图1. 离散位错动力学模拟中位错的离散化处理

Fig.1. Dislocation discretization in the discrete dislocation dynamics simulation (The red node is the physical node, representing the real dislocation node; the blue nodes are the discretization nodes, which are generated according to certain rules; the green point is the surface node, which connects a dislocation segment; the black line is the dislocation segment)Color online