A Three-Dimensional Discrete Dislocation Dynamics Simulation on Micropillar Compression of Single Crystal Copper with Dislocation Density Gradient |
||||||||||||||||
| Jian XIONG,Dean WEI,Songjiang LU,Qianhua KAN,Guozheng KANG,Xu ZHANG | ||||||||||||||||
| 表1 模型各层的位错源数量、初始位错密度与位错间距 | ||||||||||||||||
| Table 1 Number of sources, dislocation density and dislocation spacing in different layers for the model configurations | ||||||||||||||||
|
||||||||||||||||