铜绿假单胞菌对CrCoNi中熵合金微生物腐蚀行为的影响
冯浩1,李花兵1(),路鹏冲1,杨纯田2,姜周华1,武晓雷3
Investigation on Microbiologically Influenced Corrosion Behavior of CrCoNi Medium-Entropy Alloy byPseudomonas Aeruginosa
FENG Hao1,LI Huabing1(),LU Pengchong1,YANG Chuntian2,JIANG Zhouhua1,WU Xiaolei3

图3. CrCoNi中熵合金与316L不锈钢在无菌及含铜绿假单胞菌培养基中浸泡不同时间的Nyquist图和Bode图

Fig.3. Nyquist (a, c, e) and Bode (b, d, f) plots of CrCoNi MEA in sterile medium (a, b) and P. aeruginosa medium (c, d), and 316L SS in P. aeruginosa medium (e, f) for different time (Z'—real part of impedance, Z"—imaginative part of impedance, f—frequency, Z—modulus impedance)