铜绿假单胞菌对CrCoNi中熵合金微生物腐蚀行为的影响
|
|
冯浩,李花兵,路鹏冲,杨纯田,姜周华,武晓雷
|
Investigation on Microbiologically Influenced Corrosion Behavior of CrCoNi Medium-Entropy Alloy byPseudomonas Aeruginosa
|
|
Hao FENG,Huabing LI,Pengchong LU,Chuntian YANG,Zhouhua JIANG,Xiaolei WU
|
|
| 表2 CrCoNi中熵合金与316L不锈钢在无菌及含铜绿假单胞菌培养基中EIS拟合参数 |
| Table 2 Fitting parameters for EIS of CrCoNi MEA and 316L SS in sterile medium and P. aeruginosa medium |
|
| Sample | Duration | Rs | QfY | nf | Rf | QdlY | ndl | Rct | Σχ2 |
|---|
| d | Ω·cm2 | μF·cm-2·Sn | | Ω·cm2 | μF·cm-2·Sn | | 106 Ω·m2 | 10-3 | CrCoNi MEA in sterile medium | 1 | 6.73 | 20.20 | 0.93 | 13.1 | 10.40 | 0.92 | 1.22 | 0.22 | | 4 | 7.09 | 18.85 | 0.93 | 46.2 | 6.03 | 0.92 | 7.14 | 0.34 | | 7 | 7.26 | 18.20 | 0.93 | 35.6 | 6.39 | 0.91 | 9.73 | 0.41 | | 10 | 7.01 | 18.58 | 0.93 | 29.5 | 6.62 | 0.92 | 7.85 | 0.27 | | 14 | 7.34 | 18.68 | 0.93 | 41.0 | 5.97 | 0.92 | 13.46 | 0.28 | CrCoNi MEA in P. aeruginosa medium | 1 | 8.07 | 22.24 | 0.90 | 26.0 | 9.40 | 0.89 | 1.38 | 0.18 | | 4 | 6.49 | 21.79 | 0.90 | 144.2 | 5.02 | 0.91 | 0.83 | 0.74 | | 7 | 6.58 | 23.57 | 0.90 | 131.7 | 6.31 | 0.91 | 0.77 | 0.67 | | 10 | 6.73 | 20.46 | 0.91 | 195.3 | 4.15 | 0.92 | 1.14 | 0.65 | | 14 | 6.90 | 17.86 | 0.91 | 314.0 | 2.86 | 0.93 | 2.76 | 0.68 | 316 SS in P. aeruginosa medium | 1 | 5.85 | 79.50 | 0.86 | 30.9 | 41.90 | 0.85 | 0.29 | 0.64 | | 4 | 5.42 | 43.27 | 0.85 | 607.2 | 9.24 | 0.92 | 1.06 | 1.08 | | 7 | 5.85 | 52.09 | 0.85 | 521.0 | 6.17 | 0.88 | 0.55 | 0.67 | | 10 | 4.86 | 64.74 | 0.87 | 802.5 | 24.97 | 0.86 | 2.58 | 0.23 | | 14 | 4.81 | 79.43 | 0.86 | 689.3 | 26.08 | 0.86 | 1.46 | 0.17 |
|
|
|