粉末高温合金中SiO2夹杂物与基体的界面反应机理及对其变形行为的影响
冯业飞,周晓明,邹金文(),王超渊,田高峰,宋晓俊,曾维虎
Interface Reaction Mechanism Between SiO2 and Matrix and Its Effect on the Deformation Behavior of Inclusionsin Powder Metallurgy Superalloy
FENG Yefei,ZHOU Xiaoming,ZOU Jinwen(),WANG Chaoyuan,TIAN Gaofeng,SONG Xiaojun,ZENG Weihu

图4. HIP态复合夹杂物周围γ'相的SEM像

Fig.4. Low (a, c) and high (b, d) magnified SEM images of 30 μm (a, b) and 60 μm (c, d) composite inclusions after HIP