丝材+电弧增材制造钛/铝异种金属反应层的研究
|
|
Study of the Reaction Layer of Ti and Al Dissimilar Alloys by Wire and Arc Additive Manufacturing
|
|
图6. 图4a中II区的TEM分析 |
Fig.6. TEM analyses of area II in Fig.4a(a) TEM image of net shape phase (b) electron diffraction pattern of circle area in Fig.6a(c) TEM image of long strip phase (d) electron diffraction pattern of circle area in Fig.6c |
![]() |