丝材+电弧增材制造钛/铝异种金属反应层的研究
|
|
Study of the Reaction Layer of Ti and Al Dissimilar Alloys by Wire and Arc Additive Manufacturing
|
|
图7. 钛/铝反应层形成示意图 |
Fig.7. Schematic of the formation of Ti/Al reaction layer(a) interdiffusion of Ti and Al atoms (b) formation of TiAl3 in area III in Fig.4a(c) formation of TiAl3 and Al2Cu in area II in Fig.4a (d) solidification of Al alloy |
![]() |