丝材+电弧增材制造钛/铝异种金属反应层的研究
|
|
Study of the Reaction Layer of Ti and Al Dissimilar Alloys by Wire and Arc Additive Manufacturing
|
|
图5. 图4a中II区微观组织的高倍SEM像及相应的元素分布 |
Fig.5. High magnified SEM image of area II in Fig.4a (a) and corresponding element distributions for Al (b), Ti (c) and Cu (d)Color online |
![]() |