丝材+电弧增材制造钛/铝异种金属反应层的研究
|
|
Study of the Reaction Layer of Ti and Al Dissimilar Alloys by Wire and Arc Additive Manufacturing
|
|
图4. 丝材+电弧增材制造(WAAM)构件微观组织 |
Fig.4. OM image of Ti/Al wire and arc additive manufacturing (WAAM) component (a), SEM images of areas II (b), III (c) and IV (d) in Fig.4a |
![]() |