Zn添加对预时效态Al-Mg-Si-Cu合金自然时效和烘烤硬化性的影响
|
|
Effects of Zn Addition on the Natural Ageing Behavior and Bake Hardening Response of a Pre-Aged Al-Mg-Si-Cu Alloy
|
|
图8. 预时效态不含Zn和含Zn合金在自然时效和烘烤过程中的析出相演变的示意图 |
Fig.8. Schematics of precipitation evolution in the pre-aged Zn-free (a) and Zn-added (b) alloys during NA and BH treatmentsColor online |
![]() |