Zn
添加对预时效态
Al-Mg-Si-Cu
合金自然时效和烘烤硬化性的影响
朱上
1
,李志辉
1
(
),闫丽珍
1
,李锡武
1
,张永安
1
,熊柏青
1,
2
Effects of Zn Addition on the Natural Ageing Behavior and Bake Hardening Response of a Pre-Aged Al-Mg-Si-Cu Alloy
ZHU Shang
1
,LI Zhihui
1
(
),YAN Lizhen
1
,LI Xiwu
1
,ZHANG Yongan
1
,XIONG Baiqing
1,
2
图1.
热处理过程示意图
Fig.1.
Schematic of heat treatment process