交流磁场对过共晶Al-Fe合金初生相的影响
张建锋1,蓝青2,郭瑞臻2,乐启炽2()
Effect of Alternating Current Magnetic Field on the Primary Phase of Hypereutectic Al-Fe Alloy
ZHANG Jianfeng1,LAN Qing2,GUO Ruizhen2,LE Qichi2()

图6. 过共晶Al-2.55%Fe合金的XRD谱

Fig.6. XRD spectra of the hypereutectic Al-2.55%Fe alloy with (a) and without (b) alternating current magnetic field (20 Hz, 100 A)