低碳铁素体不锈钢高频直缝电阻焊管退火工艺优化
邵毅,李彦默,刘晨曦(),严泽生,刘永长
Annealing Process Optimization of High Frequency Longitudinal Resistance Welded Low-CarbonFerritic Stainless Steel Pipe
SHAO Yi ,LI Yanmo ,LIU Chenxi (),YAN Zesheng ,LIU Yongchang

图6. 退火处理后焊缝区析出相的表征

Fig.6. TEM (a), EDS (b), HRTEM (c) images and SAED pattern (d) of precipitated phase in as-annealed weld zone (d-interplanar spacing)