节约型双相不锈钢TRIP效应致塑性增量及其固溶温度依赖性
陈雷1,2,郝硕1,2,梅瑞雪2,贾伟2,李文权2,郭宝峰2()
Intrinsic Increment of Plasticity Induced by TRIP and Its Dependence on the Annealing Temperature in a Lean Duplex Stainless Steel
CHEN Lei1,2,HAO Shuo 1,2,MEI Ruixue 2,JIA Wei 2,LI Wenquan 2,GUO Baofeng2()

图7. 不同奥氏体稳定性下的本征塑性增量

Fig.7. Intrinsic plastic increment under different austenite stability