Nd含量对磁控溅射Si(111)/Cr/Nd-Co/Cr薄膜结构与磁性的影响
何贤美1,童六牛2(),高成2,王毅超2
Effect of Nd Content on the Structure and Magnetic Properties of Si(111)/Cr/Nd-Co/Cr Thin Films Prepared by Magnetron Sputtering
HE Xianmei1,TONG Liuniu2(),GAO Cheng2,WANG Yichao2

图4. 制备态Si(111)/Cr(10 nm)/NdCox(400 nm)/Cr(10 nm)薄膜的MFM像

Fig.4. Magnetic force microscopy (MFM) images for the as-deposited Si(111)/Cr(10 nm)/NdCox(400 nm)/Cr(10 nm) films with x=2.5 (a), x=3.8 (b), x=5.2 (c) and x=7.2 (d), respectively