[an error occurred while processing this directive]
低压冷喷涂制备Al(Y)-30%Al2O3涂层及其海水腐蚀行为
白杨1,2,王振华3,李相波3,李焰1()
Corrosion Behavior of Al(Y)-30%Al2O3 Coating Fabricated by Low Pressure Cold Spray Technology
BAI Yang1,2,WANG Zhenhua3,LI Xiangbo3,LI Yan1()

图1. 不同Y含量Al(Y)-30% Al2O3 (体积分数)涂层的表面形貌

Fig.1. Surface morphologies of the Al(Y)-30%Al2O3 (volume fraction) coatings with 0.05% (a), 0.1% (b), 0.2% (c) and 0.5% (d) Y (mass fraction)