SiC/2009Al复合材料的变形加工参数的优化仿真研究
马凯1,2,张星星1,王东1,王全兆1,刘振宇1,肖伯律1(),马宗义1
Optimization and Simulation of Deformation Parameters of SiC/2009Al Composites
MA Kai1,2,ZHANG Xingxing1,WANG Dong1,WANG Quanzhao1,LIU Zhenyu1,XIAO Bolv1(),MA Zongyi1

图6. 15%SiC/2009Al复合材料不同变形参数下的等效应变量随试样位置变化

Fig.6. Variations of effective strain with specimen locations from the center of the upper end to the center of the lower end (a) and from the center of the sample to the bulge (b) under different deformation parameters for 15%SiC/2009Al composite