SiC/2009Al复合材料的变形加工参数的优化仿真研究
马凯1,2,张星星1,王东1,王全兆1,刘振宇1,肖伯律1(),马宗义1
Optimization and Simulation of Deformation Parameters of SiC/2009Al Composites
MA Kai1,2,ZHANG Xingxing1,WANG Dong1,WANG Quanzhao1,LIU Zhenyu1,XIAO Bolv1(),MA Zongyi1

图5. 15%SiC/2009Al复合材料在不同变形参数下的等效应力场、最大主应力场和等效应变场分布图

Fig.5. Effective stress distributions (a~c), maximum principal stress distributions (d~f) and effective strain distributions (g~i) under different deformation parameters for 15%SiC/2009Al composite