冷却速率对包晶钢凝固过程中包晶转变收缩的影响
|
|
Influence of Cooling Rate on the Contraction of Peritectic Transformation During Solidification of Peritectic Steels
|
|
图9. 结晶器内凝固初期的冷却速率与拉速对裂纹的影响 |
Fig.9. Effect of the cooling rate and casting speed at the initial solidification in mold on the crack |
![]() |