冷却速率对包晶钢凝固过程中包晶转变收缩的影响
|
|
Influence of Cooling Rate on the Contraction of Peritectic Transformation During Solidification of Peritectic Steels
|
|
图3. 图2a中A区域的δ/γ界面分析 |
Fig.3. Image analyses of the δ/γ propagation of region A in Fig.2a |
![]() |