预氧化对Co-Al-W基高温合金高温氧化和热腐蚀行为的影响 |
||||||||||||
| 高博,王磊,宋秀,刘杨,杨舒宇,千叶晶彦 | ||||||||||||
|
Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy |
||||||||||||
| Bo GAO,Lei WANG,Xiu SONG,Yang LIU,Shuyu YANG,Akihiko CHIBA | ||||||||||||
| 表4 950-PreO预氧化Co-Al-W基高温合金在800和850 ℃腐蚀99 h后CoWO4和Al2O3层厚度 | ||||||||||||
| Table 4 Mean CoWO4 and Al2O3 scale thicknesses of Co-Al-W-based superalloy after 950-PreO treatment and hot corrosion at 800 and 850 ℃ for 99 h | ||||||||||||
|
||||||||||||