表3 Co-Al-W基高温合金的Al2O3层厚度
Table 3 Mean Al2O3 scale thicknesses of Co-Al-W-based superalloy
TreatmentPrimary stage1000 ℃ oxidation for 198 h
NPreO01.78±0.34
900-PreO0.38±0.191.70±0.36
950-PreO0.89±0.261.88±0.28
1000-LPreO1.80±0.41-