新型第三代粉末高温合金
FGH100L
的显微组织与力学性能
田甜
1
,郝志博
1
,贾崇林
2
,葛昌纯
1
(
)
Microstructure and Properties of a New Third Generation Powder Metallurgy Superalloy FGH100L
TIAN Tian
1
,HAO Zhibo
1
,JIA Chonglin
2
,GE Changchun
1
(
)
图1.
FGH100L合金的DSC曲线
Fig.1.
DSC curve of FGH100L alloy