新型第三代粉末高温合金FGH100L的显微组织与力学性能
|
|
Microstructure and Properties of a New Third Generation Powder Metallurgy Superalloy FGH100L
|
|
图6. 不同工艺态的FGH100L合金析出相形貌的SEM像和EDS分析 |
Fig.6. SEM images of precipitates of FGH100L alloy under the processing of SF (a, c, d), SF+HIP+HT (e, g, h), SF+HIP+IF+HT (i, k, l) and corresponding EDS analyses (b, f, j) (Insets show the enlarged views) |
![]() |