新型第三代粉末高温合金FGH100L的显微组织与力学性能
|
|
Microstructure and Properties of a New Third Generation Powder Metallurgy Superalloy FGH100L
|
|
图5. 不同工艺态的FGH100L合金显微组织OM像 |
Fig.5. OM images of FGH100L alloy under the processing of SF (a), SF+HIP+HT (b), SF+HIP+IF+HT (c, d) (Insets show the enlarnged views) |
![]() |