成分梯度对激光沉积制造TC4/TC11连接界面组织和性能的影响
|
|
Effect of Composition Gradient on Microstructure and Properties of Laser Deposition TC4/TC11 Interface
|
|
图6. 不同过渡层数的固溶时效态TC4/TC11钛合金拉伸断口形貌的SEM像 |
Fig.6. Low (a1~c1) and locally high (a2~c2) magnified tensile fracture SEM images of solution-ageing treated TC4/TC11 alloys with transition layers 0 (a1, a2), 1 (b1, b2) and 3 (c1, c2) |
![]() |