Effect of Composition Gradient on Microstructure and Properties of Laser Deposition TC4/TC11 Interface
|
|
图4. 过渡区为3层时不同热处理制度下激光沉积制造TC4/TC11钛合金过渡区显微组织的OM像 |
Fig.4. OM images of laser deposition manufacturing TC4/TC11 alloys with 3 transition layers under heat treatment processes of No.1 (a), No.2 (b), No.3 (c), No.4 (d) and No.5 (e) |
![]() |