成分梯度对激光沉积制造TC4/TC11连接界面组织和性能的影响
|
|
Effect of Composition Gradient on Microstructure and Properties of Laser Deposition TC4/TC11 Interface
|
|
图2. 过渡区为0层时不同热处理制度下激光沉积制造TC4/TC11钛合金过渡区显微组织的OM像 |
Fig.2. OM (a, c~f) and SEM (b) images of laser deposition manufacturing TC4/TC11 alloys with 0 transition layer under heat treatment processes of No.1 (a, b), No.2 (c), No.3 (d), No.4 (e) and No.5 (f) (Curves show the TC11/TC4 interfaces) |
![]() |