可时效强化Mg-Sn基合金的研究进展
|
|
Research Progress in Age-Hardenable Mg-Sn Based Alloys
|
|
图2. Mg/Mg2Sn固态相变系统中Δg平行法则和列匹配示例 |
Fig.2. An example of Δg parallelism and row matching in Mg/Mg2Sn solid-state phase transformation system |
![]() |