变形参数对2195 Al-Li合金动态再结晶的影响
李旭,杨庆波,樊祥泽,呙永林,林林,张志清

Influence of Deformation Parameters on Dynamic Recrystallization of 2195 Al-Li Alloy
Xu LI,Qingbo YANG,Xiangze FAN,Yonglin GUO,Lin LIN,Zhiqing ZHANG
图1 试样分析位置
Fig.1 Schematic of observing areas (RD, TD, ND represent rolling, transverse and normal directions, respectively; EBSD—electron backscatter diffraction; TEM—transmission electron microscope)